This method covers preparation of specimens and the measurement of the change of diametral tensile strength resulting from the effects of water saturation and accelerated water conditioning, with a freeze-thaw cycle, of compacted asphalt mixtures. The results may be used to predict long-term stripping susceptibility of the asphalt mixtures and evaluate liquid anti-stripping additives that are added to the asphalt binder or pulverulent solids, such as hydrated lime or portland cement, which are added to the mineral aggregate.