1.1This specification covers iron-chromium-nickel, high-alloy tubes made by the centrifugal casting process intended for use under pressure at high temperatures.
1.2The grades of high alloys detailed in Table 1 are intended for applications requiring strength and resistance to corrosion and scaling at high temperatures.
1.3Optional Supplementary Requirements S1 to S11 are provided; these call for additional tests to be made if desired.
1.4The values stated in either SI units or inch-pound units are to be regarded separately as standard. The values stated in each system may not be exact equivalents; therefore, each system shall be used independently of the other. Combining values from the two systems may result in non-conformance with the standard.
1.4.1Within the text, the SI units are shown in brackets.
ASTM A608/A608M-14 History
ASTM A608/A608M-14
$30.00 $60.00
ASTM A608/A608M-06(2012)
$30.00 $60.00
More Standards PDF
ASTM D7549-23
$54.00 $108.00
ASTM D2322-14(2023)
$25.00 $50.00
ASTM D6947/D6947M-16(2023)
$25.00 $50.00
ASTM D6224-23
$34.00 $69.00