This specification covers a corrosion and heat resistant nickel alloy in the form of investment castings.
These castings have been used typically for parts, such as nozzle guide vanes, requiring high strength up to 1500 degrees F (816 degrees C) and oxidation resistance up to 1800 degrees F (982 degrees C), but usage is not limited to such applications.
These castings have been used typically for parts, such as nozzle guide vanes, requiring high strength up to 1500 degrees F (816 degrees C) and oxidation resistance up to 1800 degrees F (982 degrees C), but usage is not limited to such applications.