This specification covers a high strength, corrosion and heat resistant cobalt-chromium-nickel alloy in the form of bars.
These bars have been used typically for applications requiring a combination of high strength up to 1100 degrees F (593 degrees C), good tension-tension fatigue strength, toughness, and ductility, but usage is not limited to such applications. This alloy exhibits exceptionally good resistance to corrosion, crevice-corrosion, stress-corrosion cracking, and elevated temperature relaxation.
These bars have been used typically for applications requiring a combination of high strength up to 1100 degrees F (593 degrees C), good tension-tension fatigue strength, toughness, and ductility, but usage is not limited to such applications. This alloy exhibits exceptionally good resistance to corrosion, crevice-corrosion, stress-corrosion cracking, and elevated temperature relaxation.
SAE AMS5841E History
More Standards PDF
SAE AIR4846A
$75.00 $150.00
SAE ARP4001B
$39.00 $79.00
SAE J1693_201204
$43.00 $87.00
SAE AS50861/6
$42.00 $85.00