Dendrite Arm Spacing of Structural Aircraft Quality D357 Aluminum Allow Castings, Determination and Acceptance of

SAE International , 08/22/2018

Publisher: SAE

File Format: PDF

$37.00$74.00


This document covers the recommended practice for determining the acceptability of the dendrite arm spacing (DAS) of D357-T6 aluminum alloy castings required to have tensile strength not lower than 50000 psi (345 MPa).